Printing for Packaging: Processes, Colour, Finishing
A working reference to packaging print: the six processes and when each fits, prepress rules, colour targets, board and ink choice, finishing and costs.

Printing is where a packaging project stops being an idea and becomes a manufactured object. Almost every reprint, late shipment and colour dispute traces back to a decision that was made — or skipped — before the press started: a dieline that ignored bleed, a spot colour converted to process without approval, a laminate applied over ink that had not fully cured, or a crease line set for the wrong board caliper.
This reference is a single working overview of that chain. It covers the six print processes used on packaging, how to match one to a run length and substrate, the prepress rules that decide whether a file prints cleanly, colour targets and proofing routes, board and ink selection, finishing operations and how they interact, quality control from first sheet to final carton, the cost structure behind a quotation, and the compliance points that reliable suppliers check before shipping. It is written for buyers, brand owners and product engineers who need to specify a job with enough precision that two suppliers quote the same thing.
Use it as a map. Where a topic deserves its own depth, this site's dedicated guides cover dieline file preparation, colour management, print finishes, labels and food-contact compliance.
The six printing processes used for packaging
Packaging print is not one technology. The process determines minimum run length, achievable detail, colour stability across the run, substrate tolerance and unit price. Choosing it is the first decision, and reversing it later usually means new tooling.
Offset lithography
Offset prints from a thin aluminium plate (typically 0.15–0.3 mm) onto a rubber blanket and then onto the sheet. Ink transfers only where the plate is image-bearing, so the process combines fine detail with high output speed. Sheetfed presses handle stock from about 60 g/m² up to 600 g/m² card, and large-format machines print sheets of 70 × 100 cm and above, which is why most folding cartons are produced several up per sheet.
- Typical screen ruling: 60–80 lines/cm (150–200 lpi) on coated board; finer rulings need better stock and tighter process control.
- Strengths: fine type and gradients, dense solid coverage, repeatable colour over long runs, spot colours plus varnish in one pass.
- Limits: plate and make-ready cost make very short runs expensive; thick rigid board above roughly 1.5 mm is normally printed flat and wrapped rather than printed directly; each additional colour adds a unit and a plate set.
- Typical use: folding cartons, litho-laminated corrugated (offset-printed liner glued to board), labels, sleeves, rigid box wrap paper.
Flexography
Flexo uses a photopolymer relief plate mounted on a cylinder, inked by an anilox roll whose engraved cells meter a fixed ink film. It prints on a wide range of substrates, including corrugated board, kraft, film and label stock, with water-based, solvent or UV inks.
- Anilox specification drives the job: roughly 200–800 lines per inch (80–320 lines per cm) with cell volumes of about 2–12 cm³/m².
- Strengths: economical at volume on absorbent stock, robust on rough surfaces, lower plate cost than gravure, capable of in-line die-cutting and gluing.
- Limits: dot gain is higher than offset and must be compensated in prepress; fine reverse type and long gradients need care; colour drift across a long corrugated run is more visible than on coated card.
- Typical use: corrugated shipping and retail-ready cases, kraft mailers, labels, flexible film, bags.
Rotogravure
Gravure engraves the image into a copper cylinder, then chrome-plates it. Ink fills the cells and transfers under pressure. The process is expensive to set up — one cylinder per colour — and very stable once running.
- Strengths: consistent colour across millions of impressions, strong performance on thin films and metallised substrates, smooth tone reproduction.
- Limits: cylinder cost and lead time (commonly 5–15 days) make it unsuitable at low volume; artwork changes mean new cylinders; cylinders need storage.
- Typical use: flexible packaging, shrink sleeves, high-volume labels, decorative laminates.
Digital toner printing
Electrophotographic presses build the image from charged toner particles, typically at 600–1,200 dpi, with no plates and no make-ready.
- Strengths: economical from one unit to a few thousand, versioning and variable data without extra tooling, fast turnaround, consistent output between runs.
- Limits: stock range is narrower (many devices cap around 350–400 g/m²), spot colours are simulated unless the press has extra stations, toner sits on the surface so scuff resistance on uncoated stock is lower than offset, and large solids can show banding.
- Typical use: short-run cartons, prototypes, sample packs, personalised labels and sleeves.
Digital inkjet
Piezo printheads jet ink droplets of roughly 2–12 pL in water-based, UV-curable or latex formulations. Single-pass machines print corrugated sheets directly; wide-format machines handle prototypes, displays and short-run rigid work.
- Strengths: no tooling, wide format, direct-to-board printing, extended gamut with added orange or violet inks, practical for versioned or regional packaging.
- Limits: cost per square metre is higher than offset or flexo at volume; ink coverage limits on absorbent board; colour gamut and gloss depend heavily on substrate and coating.
- Typical use: sample and e-commerce packaging, short-run corrugated, promotional displays, proofing on production board.
Screen printing
Screen printing pushes ink through a mesh, depositing a thick, opaque film — commonly 10–30 µm wet.
- Strengths: high opacity on dark or transparent stock, strong whites, metallic and special-effect inks, suitable for glass, plastic, rigid boxes and similar surfaces.
- Limits: coarse detail, lower speed, colour count limited by stations; not suited to photographic imagery.
- Typical use: cosmetic rigid boxes, glass and tube decoration, spot whites on transparent film, special effects.
Processes used for decoration rather than full colour
Letterpress and hot-foil stamping are still used, but as finishing operations rather than primary print: they deliver tactile impressions and metallic effects that ink alone cannot reproduce. Litho lamination — printing a liner by offset and laminating it to corrugated board — sits between processes and is the standard route when a corrugated case needs offset quality on the outside.
Matching a process to run length, substrate and colour
Most sourcing errors come from choosing a process by habit. The practical sequence is to fix the substrate and the run length first, then let those two narrow the options.
- Under about 500 units: digital toner or inkjet, unless a specific effect (foil, window, unusual board) forces a conventional route with fixed tooling.
- 500–5,000 units on coated card: offset becomes competitive once plates and make-ready are amortised; digital still wins when versioning or speed matters.
- 5,000–100,000 units: offset for cartons, flexo for corrugated and labels; gravure enters for film and very high volumes.
- Above 200,000 units on film or metallised stock: gravure or high-end flexo, judged on colour stability rather than unit price alone.
- Rough, absorbent or recycled stock: flexo handles it better than offset; offset needs a coated surface and tighter moisture control.
- Food-contact primary packaging: any process is viable, but inks, coatings and adhesives must be selected for low migration and the whole chain documented.
- More than six colours or heavy special effects: conventional printing with spot units, because digital spot simulation rarely matches a brand colour on a textured board.
Two practical rules of thumb: adding a spot colour typically lifts unit price by a few percent on mid-size runs and much more on short ones; doubling run length usually reduces unit price by 15–30% because make-ready and waste are spread over more units.
Prepress: the file work that decides whether the job prints
Prepress is where most money is saved or lost, because every correction at this stage costs minutes and every correction after plating costs hours.
- Dieline on its own layer, at 100% scale, never scaled or rotated. Cut, crease, perforation and glue-flap lines must be distinguishable and named consistently.
- Bleed of at least 3 mm beyond trim on every edge that reaches the cut, and 5 mm where a fold sits close to the trim. Artwork that stops at the dieline shows a white sliver after die-cutting.
- Safe area of 3–5 mm inside the trim and crease lines for all text and critical graphics; more where a window or hang tab intrudes.
- Image resolution of 300 ppi at final printed size, 1,200 dpi for 1-bit line art and barcodes. Upsampling a low-resolution web image does not create detail.
- Vector logos and type over 6 pt, ideally 7 pt or more for reverse type on dark solids. Four-colour small type is prone to registration fringing; use a single spot or black instead.
- Embedded fonts or outlined type, transparency flattened correctly, and delivery as PDF/X-4 — the exchange format that keeps colour and overprint intent intact.
- Spot colours named exactly as the ink will be ordered (for example PANTONE 186 C), used identically across pages, and never recreated by converting a process build.
- Overprint set deliberately: black text overprinting where appropriate, white knocked out where it must stay clean, and trapping of about 0.05–0.2 mm where two colours meet on a moving substrate.
- Total area coverage within press limits — typically 300–340% on coated sheetfed work — to avoid set-off, poor drying and blocking.
- Barcodes: EAN-13 at 80–200% magnification, with the required quiet zones (about 3.63 mm left and 2.31 mm right for EAN-13), bar width reduction matched to the process, and no barcode placed across a crease or on a curved surface.
- Imposition planned around the gripper area (about 8–10 mm) and sheet efficiency; grain direction parallel to the main fold so cartons do not crack or warp.
- Print-ready delivery also means a colour reference: a contract proof, or a previously approved printed sample on the same stock.
Colour: targets, measurement and approval
Colour is the most negotiated and least objective part of packaging print, so the job needs a written target rather than an opinion.
CMYK, spot and extended gamut
Process colour builds images from cyan, magenta, yellow and black. Spot colour is a pre-mixed ink matched to a reference — the way to hold a brand colour on a given stock. Extended-gamut printing adds orange, green or violet to reach colours CMYK cannot, at the cost of more units and a more complex profile. Converting a spot colour to CMYK is a commercial decision with a technical consequence: it changes the achievable colour, especially on uncoated and recycled board, and needs written approval against a proof.
Targets and tolerances
- Offset printing follows ISO 12647-2 process control: defined ink film, dot gain and substrate-dependent targets rather than one master colour.
- Dot gain at 50% typically lands at 12–20% depending on stock and press; prepress curves must compensate or mid-tones print dark and muddy.
- Colour difference is judged with ΔE: ΔE00 of 1.0–2.0 is generally acceptable for brand work, 2.0–3.0 is visible side by side, and above 3.0 usually triggers rejection.
- Measurement follows ISO 13655 conditions (M1 illumination for today's optical brighteners), with the same instrument and the same backing used for approval.
- Rich black builds (for example 60/40/40/100) are specified where large black areas need density; registration black is reserved for line work, never for large fills.
- Metallic and fluorescent inks cannot be matched by process simulation; their lightfastness and rub behaviour differ from standard inks and should be agreed explicitly.
Proofing routes
- Soft proof: calibrated display plus an ICC profile of the target press and stock. Useful for layout, insufficient for colour approval.
- Contract proof: printed on a proofing device to ISO 12647-7 tolerances, on a substrate that simulates the production board. This is the normal approval document.
- Press proof: a short run on the actual press before the full run. Reserved for brand-critical work, difficult colours and new substrates.
- Viewing conditions matter: ISO 3664 D50 illumination at around 2,000 lx. Approving a proof in an office lit by warm LED downlights is a reliable way to reject a good print.
Screening and image reproduction
Halftone screening converts continuous tone into printable dots. The choice affects perceived sharpness, stability and the risk of interference patterns.
- AM screening with a fixed ruling of 60–80 lines/cm is the standard for coated cartons; finer rulings improve detail but demand better stock and tighter register.
- FM (stochastic) screening uses small randomly placed dots, holding detail without a visible rosette but stressing plate and press cleanliness.
- Hybrid screening keeps AM dots in mid-tones and switches to FM in highlights and shadows, a common compromise for packaging.
- Moiré appears when screen angles conflict with a printed pattern, a woven texture or a window mesh. Keeping screen angles about 30° apart and avoiding overlaid fine patterns reduces the risk.
- Solid ink density, dot gain and register are controlled from colour bars in the trim area; without them a run can be judged but not measured.
Substrates: what the press needs from the board
Board choice sets the achievable colour, the fold behaviour and the cost floor. Grammage, caliper and bulk are different properties and cannot be substituted for one another.
- Grammage in g/m² (ISO 536) describes mass; caliper in µm (ISO 534) describes thickness; bulk in cm³/g is the ratio that shapes stiffness feel. A 300 g/m² board at 1.6 cm³/g behaves differently from the same grammage at 1.25 cm³/g.
- Coated one side, coated two sides and uncoated surfaces print differently: coated stock holds fine detail and gloss, uncoated absorbs ink and shifts colour warmer and duller.
- FBB (folding boxboard) offers high bulk and good creasing for cartons; SBS (solid bleached board) gives a bright white print surface for premium work; coated recycled board is economical but shows more colour variation and needs a low-migration assessment for food.
- Moisture content of 5–8% (ISO 287) is the working range; board that is too dry cracks at the crease, board that is too damp warps and misregisters.
- Grain direction must run parallel to the main fold. Folding against the grain produces hairline cracks through the printed surface, immediately visible on dark solids.
- Whiteness and opacity change ink appearance more than many buyers expect; a brand colour approved on SBS looks different on recycled board with a lower white point.
- Storage matters: about 20 ± 5 °C and 50 ± 10% relative humidity, with 24 hours of conditioning before printing, prevents wavy edges and feeding problems.
- Fibre sourcing is documented through chain of custody: FSC-STD-40-004 V3-1 or PEFC certification, with the claim and label artwork matching the certificate scope.
Inks and coatings
Ink selection is a functional decision for packaging, not only an aesthetic one. The ink must adhere, resist rub and light, survive converting and — for food contact — not migrate into the product.
- Conventional offset inks are mineral-oil or vegetable-oil based and dry by absorption and oxidation; they need spray powder and time before finishing.
- UV and LED-UV inks cure instantly under lamps, allowing same-day finishing on non-absorbent stock, but they sit higher on the surface and change the feel of the sheet.
- Water-based flexo inks suit absorbent board and corrugated; solvent inks hold out better on film.
- Low-migration ink systems, produced under EuPIA good manufacturing practice, are the normal choice for primary food packaging, supported by a statement of compliance and migration testing where required.
- Metallic inks based on bronze or aluminium particles oxidise and lose brilliance unless protected by varnish or laminate; fluorescent inks have limited lightfastness and are unsuitable for long-life packaging.
- Lightfastness is rated on the Blue Wool scale (1–8); retail packaging exposed to daylight needs higher ratings than a carton that ships inside an outer case.
Coatings fall into a few families and are often combined:
- Aqueous varnish: 1–3 g/m², matt or gloss, economical scuff protection, overprintable and fibre-recyclable.
- UV varnish: 3–8 g/m², high gloss or matt, applied full or spot; spot UV over a matt laminate is the classic contrast effect and depends on registration.
- Lamination: BOPP at about 12–18 µm or PET at about 12–23 µm, matt, gloss or soft-touch. It gives the highest scuff and moisture resistance and the strongest tactile signal, at the cost of recyclability in some fibre streams.
- Window film: PET, from around 12 µm for small patches to 0.3 mm for large structural windows, chosen by panel size, clarity and puncture resistance.
Postpress: converting and finishing
Finishing turns printed sheets into a package, and each operation adds its own tolerance stack. Tolerances that are individually acceptable can combine into a misfit.
- Die-cutting uses steel rules in a plywood forme; typical positional tolerance is ±0.2–0.3 mm, with nicks holding the carton in the sheet until stripping.
- Creasing is set from board caliper: crease rule, matrix channel and counter are matched so the fold compresses rather than tears the board. Incorrect crease geometry is the most common cause of cracking on laminated stock.
- Hot-foil stamping runs at roughly 100–150 °C with a dwell of 0.3–1 s; release depends on foil grade, stock smoothness and pressure. Cold foil uses adhesive plus UV cure and suits finer detail at higher speed.
- Embossing and debossing use matched male and female dies, typically 0.3–0.8 mm deep; multi-level dies add sculpted detail at extra tooling cost.
- Window patching applies film over an aperture with adhesive; wrinkle and haze are the two failure modes to inspect.
- Gluing covers side-seam, crash-lock and four- or six-corner styles; bond strength is judged by fibre tear, not by how hard the flap resists.
- Rigid boxes wrap grey board (commonly 1.0–3.0 mm) in printed paper of 100–157 g/m²; corner turnover, joint gap and lid fit define perceived quality more than print does.
- Book and booklet work adds saddle stitching, perfect binding with PUR or EVA, and mechanical binding, each with its own minimum extent and spine tolerance.
How finishing steps interact, and where jobs fail
Finishing steps are not independent. Most finishing faults are conflicts between two operations, and the fix usually sits earlier in the chain.
- Laminating over heavy ink coverage traps solvent and causes bubbles or delamination; reduce ink film, add drying time, or use UV inks.
- Foiling onto a laminated or heavily varnished surface fails to anchor; foil needs a receptive surface, so the sequence is often print, laminate, then foil with a compatible foil grade.
- Spot UV over matt laminate requires registration within about ±0.3 mm; thin outlines around the gloss area show any drift.
- Creasing through laminated board cracks unless crease width is widened and the board conditioned; grain direction and caliper decide whether it works.
- Gluing on a coated or laminated surface fails when adhesive cannot key; the glue flap is often left uncoated, or a hot-melt is specified.
- Stacking printed sheets too high before drying causes set-off and blocking, especially with matt inks and dense solids.
- Die-cutting after lamination can delaminate at the cut edge if the laminate bond is weak; bond strength is verified before the run, not after.
Quality control from first sheet to final carton
A print job is approved in stages, and each stage needs its own evidence. Suppliers who can show these records consistently deliver fewer surprises.
- First-off approval: the first good sheet or carton is signed against the approved proof, under the specified viewing conditions, before the run continues.
- Colour control: density and ΔE measurements from colour bars at start, middle and end of the run, recorded against the target.
- Register and print defects: in-line camera inspection or operator checks for hickies, scumming, ghosting and misregistration.
- Barcode verification: graded against ISO/IEC 15416, with a minimum grade of 1.5 (C) commonly required by retailers; the grade depends on contrast, bar width growth and quiet zones.
- Surface performance: rub resistance (ASTM D5264), ink adhesion by tape test (ASTM D3359), laminate bond by peel test (FINAT FTM 2).
- Structural checks: dimensions against the dieline, glue bond by fibre tear, window clarity, lid fit on rigid boxes.
- Sampling: incoming and final inspection to ISO 2859-1, commonly General Inspection Level II with AQL 2.5 for major and 4.0 for minor defects.
- Transit validation: ISTA 1A for single packages and 2A or 3A for parcel and less-than-truckload distribution, or ISO 12048 compression for stacked pallets.
- Retained samples: a signed reference from each run, kept for at least the reorder window, so a repeat order is matched to a physical standard rather than a memory.
- Documentation: statement of compliance for food-contact work, chain-of-custody certificate for fibre claims, and a deviation report for anything accepted outside tolerance.
Cost structure: what actually drives the quotation
Unit price is a thin slice of the real cost model, and comparing quotations without that model is how buyers choose a supplier that cannot deliver the price twice.
- Tooling: plates, cutting dies, foiling dies, embossing dies, screen frames and gravure cylinders. Tooling is usually quoted separately and may be charged again on artwork changes.
- Make-ready: press set-up, ink matching, registration and waste sheets. A short run carries nearly the same make-ready as a long one, which is why unit price falls sharply with volume.
- Substrate: typically the largest single line for cartons, at roughly 40–60% of unit cost depending on grade and board weight.
- Colour count: each additional unit adds plates, ink, make-ready time and waste; specials such as metallic, fluorescent or low-migration inks add more.
- Finishing: lamination, foiling, embossing, windowing and gluing each carry set-up plus running cost, and each adds handling between operations.
- Spoilage allowance: production plans normally include a few percent over the ordered quantity, and trade tolerances on over- or under-delivery are common.
- Freight: chargeable weight is the greater of actual weight and volume weight, using a divisor of roughly 5,000–6,000 cm³/kg by mode and carrier; flat-packed cartons ship far more cheaply than assembled ones.
- Terms: Incoterms 2020 determines where cost and risk transfer; ex-works quotations exclude freight, insurance and destination charges that appear later.
- Payment and MOQ: deposits, balance terms and minimum order quantities change the effective cost of capital, especially on repeat programmes.
- Engineering changes: artwork revisions after plates or dies are made typically trigger re-tooling plus a new make-ready.
Compliance and sustainability for printed packaging
Regulatory exposure sits in the ink, the coating, the adhesive and the fibre — not only in the finished appearance.
- Food contact: EU Regulation (EU) No 10/2011 sets an overall migration limit of 10 mg/dm² for plastic layers, with specific limits per substance; FDA 21 CFR 175.300 covers resinous and polymeric coatings and 21 CFR 176.170 covers paper and paperboard components; GB 4806.1-2016 with GB 4806.7-2016 and GB 4806.8-2016 governs food-contact plastics and paper in China.
- Non-intentionally added substances (NIAS) must be assessed for food-contact printing, and low-migration inks, coatings and adhesives are documented through statements of compliance.
- Mineral oil hydrocarbons (MOSH/MOAH) are a known risk with recycled fibre and conventional offset inks; functional barriers or virgin-fibre food-contact layers are the usual mitigations.
- Heavy metals: EU Directive 94/62/EC limits the combined content of lead, cadmium, mercury and hexavalent chromium to 100 mg/kg in packaging and packaging components; the CONEG model legislation applies a similar limit in several US states.
- Toys and child-related packaging: EN 71-3 migration limits apply to accessible materials, and inks and coatings must be assessed accordingly.
- Fibre claims: FSC-STD-40-004 V3-1 chain of custody, or the equivalent PEFC standard, must cover the mill and every handler in the chain that changes the claim.
- Recyclability: repulpability and deinking behaviour depend on coating weight, laminate type and ink chemistry. Full-surface PET lamination and metallised film usually take a carton out of standard fibre recycling.
- PFAS restrictions are evolving across jurisdictions; suppliers should confirm current status for grease-barrier coatings rather than relying on legacy approvals.
- Volatile organic compounds and energy use are controlled through ink selection (water-based, UV) and press emissions abatement, and increasingly appear in customer sustainability questionnaires.
Twenty failure modes and how to prevent them
- Colour drift between proof and press: substrate, ink and profile not matched — approve on a proof that simulates the production board.
- Ghosting in solids: ink starvation or blanket problems — check ink feed and blanket condition, move heavy solids away from light areas.
- Hickies: dried ink, paper dust or coating particles — filter ink, clean blankets, check board surface.
- Scumming: dampening imbalance or plate contamination — reset fountain solution, check plate and roller settings.
- Set-off and blocking: insufficient drying or over-stacked sheets — reduce pile height, add anti-set-off spray, delay finishing.
- Excessive dot gain: impression pressure, ink film or a soft blanket — recalibrate, adjust curves.
- Misregistration: paper stretch, wrong gripper, humidity — condition stock, check gripper and register marks.
- Moiré: conflicting screen angles or a printed pattern — change angles or screening method.
- Poor ink adhesion on coated stock: surface energy below about 38 dyn/cm — corona treat, prime, or specify a compatible ink.
- Foil not releasing: temperature, pressure or dwell off target, or stock too rough — adjust parameters, add primer, choose a finer foil.
- Lamination bubbles or delamination: solvent trapped in ink, weak adhesive — reduce ink film, add drying, verify bond.
- Crease cracking: wrong crease geometry, grain across the fold, board too dry — widen the crease, re-cut with correct grain, condition the board.
- Die-cut misregistration: sheet stretch or wrong pin position — check gripper, adjust the forme.
- Glue failure: coated surface or short compression — leave a glue flap uncoated, increase compression time, specify hot-melt.
- Window wrinkle or haze: film tension and adhesive — adjust patching tension, verify film grade.
- Warp and curl: moisture imbalance or one-side coating — condition board, balance coating, control stacking.
- Odour or taste taint: solvent residue or an unsuitable ink — specify low-odour or low-migration systems, allow full cure.
- Barcode grade failure: bar width growth, low contrast or a blocked quiet zone — apply bar width reduction, keep the background light and clear.
- Scuffing in transit: no protection on a matt surface — add varnish or laminate, use interleaving.
- Migration into food: conventional ink on a food-contact surface without a barrier — switch to a low-migration system or add a functional barrier.
Approving a print job: a practical checklist
- Dieline, artwork and varnish plates all at 100% scale and version-matched.
- Bleed, safe area, overprint and trapping checked on the final PDF, not on a screenshot.
- Spot colours named to the ink that will be ordered, with process conversions approved in writing.
- Contract proof approved on simulated production stock, viewed under D50 illumination.
- Board grade, grammage, caliper and certification stated on the purchase order.
- Ink system confirmed as standard or low-migration, with the statement of compliance attached.
- Finishing sequence agreed in writing, including which surface each effect applies to.
- Crease and fold behaviour demonstrated on the actual board before the full run.
- Colour and barcode measurement criteria written into the order, with acceptance limits.
- Sampling plan, AQL levels and inspection level agreed before production.
- Transit test requirement stated, with the ISTA procedure reference.
- Delivery tolerance, over/under allowance and the packaging of the cartons themselves specified.
- Signed reference sample retained by both parties for the reorder window.
- Change control: any artwork or material change re-quotes tooling and lead time.
Key figures and tolerances
- Dot gain at 50%: 12–20% depending on stock and process (ISO 12647-2)
- Total area coverage: 300–340% for coated sheetfed board (ISO 12647-2)
- Colour difference: ΔE00 1.0–2.0 acceptable, above 3.0 usually rejected (ISO 13655)
- Registration tolerance: ±0.1–0.2 mm between units (ISO 12647-2)
- Board grammage and caliper: 200–450 g/m² (ISO 536), 250–600 µm (ISO 534), moisture 5–8% (ISO 287)
- Surface gloss: matte 5–15 GU, satin 25–45 GU, gloss 60–80 GU (ISO 2813)
- Barcode quality: grade 1.5–4.0 (ISO/IEC 15416) at 80–200% magnification (ISO/IEC 15420)
- Inspection sampling: AQL 2.5 major / 4.0 minor at General Inspection Level II (ISO 2859-1)
- Transit performance: ISTA 1A, 2A or 3A by distribution mode, or ISO 12048 compression for stacked loads
- Ranges are typical industry values for the material or process named and are not a specification; confirm the exact value, the current edition of each standard and the applicable grade with your supplier or test laboratory.
About this guide
Written and reviewed by the pkgoutside Editorial Team, which covers printing, packaging materials, formats and sourcing. Guides draw on supplier specifications, published industry standards and the questions buyers ask on pkgoutside. Specifications vary by supplier and market, so confirm the final material, certificates and samples with your supplier before ordering.
- Written by:
- pkgoutsideEditorial Team — packaging and print sourcing coverage
- Technical review:
- Cross-checked against the standards listed below
- Figures:
- Typical ranges for the material and process described, not a specification
- Last reviewed:
- 2026-10-31
Standards & references
The figures, test methods and compliance terms cited in this guide follow the published standards below. Editions and applicability vary by material, market and supplier, so confirm the current edition and the exact grade or specification with your supplier or test laboratory before ordering.
ISO 12647-2:2013 — Process control for half-tone colour separations, proof and production prints — offset lithography
Tone value increase (dot gain, %), solid ink density and register tolerances.
ISO 2813:2014 — Paints and varnishes — determination of gloss value at 20°, 60° and 85°
Gloss value (GU), the measurement behind matte, satin and gloss specifications.
ISO 13655:2017 — Graphic technology — spectral measurement and colorimetric computation
Measurement conditions (M0–M3) and ΔE colour tolerances for press approval.
EuPIA Guideline — Printing inks applied to the non-food contact surface of food packaging
Composition and exclusion limits for inks and coatings on food packaging board.
Source: https://pkgoutside.com/insights/printing-for-packaging-complete-reference ·pkgoutside — printing and packaging B2B marketplace. Export or archive this copy together with the URL above so readers can trace the original guide and its current version.
Related reading: Paperisation of Packaging: Designing Fibre-Based Packs That Repulp, EU PPWR Compliance: A Packaging Buyer's Document and Design Checklist, Mono-Material Flexible Packaging: Designing Packs That Recyclers Accept
More guides

Paperisation of Packaging: Designing Fibre-Based Packs That Repulp

EU PPWR Compliance: A Packaging Buyer's Document and Design Checklist

Mono-Material Flexible Packaging: Designing Packs That Recyclers Accept
More in Printing & Finishing
View all in Printing & Finishing
Colour Management for Packaging Print: Pantone and CMYK
Spot colours, CMYK process builds and brand consistency: how to set colour targets, approve proofs and control variables that move colour in production.
BypkgoutsideEditorial TeamUpdated 2026-10-24
Artwork and Dieline File Preparation: A Buyer's Checklist
Most packaging delays begin with artwork files. Here is what to prepare and check before sending print-ready files to a supplier.
BypkgoutsideEditorial TeamUpdated 2026-10-23
Printing Finishes: Matte, Gloss and Soft-Touch
Matte, gloss, soft-touch and spot UV compared, with guidance on how each finish affects feel, durability, scuff resistance and unit cost.
BypkgoutsideEditorial TeamUpdated 2026-10-22
Keep reading on the same standards